Amfani da samfurin
————————————————————
Injin gwajin zafin jiki mai tsawo na lantarki ya cika buƙatun GB / T2039-1997 "Hanyar gwajin zafin jiki mai tsawo da na tsawo na ƙarfe", HB5151-1996 "Hanyar gwajin zafin jiki mai tsawo na ƙarfe", wanda aka fi amfani da shi don gwajin zafin jiki mai tsawo, gwajin zafin jiki mai tsawo da gwajin zafin jiki mai tsawo, gwajin zafin jiki mai tsawo, gwajin zafin jiki mai tsawo, gwajin zafin jiki mai tsawo, gwajin zafin jiki mai tsawo, gwajin zafin jiki mai tsawo, gwajin zafin jiki mai tsawo. Yana da yau da kullun amfani da kayan aiki na karafa sashen, kimiyya bincike cibiyoyin, ingancin dubawa sashen, sararin samaniya, motoci masana'antu, inji masana'antu, petrochemical, gini kayan aiki, mafi girma jami'o'i da kuma m ma'adinai kamfanoni gudanar da kayan aiki dubawa da bincike.
Kayayyakin Features
————————————————————
Cika ka'idoji:
HB: 5151-1996 HB: 5150-1996 GB / T2039-2012 GB / T6395-1986 GN / T4338-2006 da sauran ka'idoji don gwaji.
Basic ayyuka:
Wannan tsarin software ne high amintacce, m aiki, kwanciyar hankali, m fadada, akwai nau'ikan rufe madauki sarrafawa hanyoyin, sigogi saiti da sarrafawa aiki ne mai sauki, abin dogaro, mai sassauci dubawa, yafi amfani da creep shakatawa m gwaji inji.
samfurin hotuna
————————————————————

Babban sigogi
————————————————————
| Bayani Model |
RMT jerin |
| Daidaito Rating |
Matsayi 0.5 |
| Max gwajin ƙarfi |
100kN |
| Gwajin ƙarfin ƙuduri |
1/500000 na matsakaicin gwajin ƙarfi, ba a rarraba shi ba, kuma ƙuduri ba ya canzawa |
| jawo bar tafiya |
≥200mm |
| sama da ƙasa clip eccentricity |
≤8% |
| Range na ma'auni na deformation |
0~10mm |
| Stretch gudun |
0~100mm/min |
| zafin jiki range | 200~1200℃ |
| Matsakaicin Tropical tsawon | ≥180mm |
| Girman baƙi |
800*500*2200mm |
Zaɓi Tristar . kyakkyawa. AmintacceCi gaba ta hanyar kirkire-kirkire, amfani ga gudanarwa
-
-
Deep fasaha tarawa
Fiye da shekaru 10 kwarewa tawagar, samun 3 inventions patents, 18 amfani model patents, 6 software ayyuka, duka da kwarewa da kuma kirkire-kirkire iya.
-
-
Gudanar da ERP
Cikakken ERP management, inganta management tsari, abubuwa sarrafawa daidai a lokaci, tabbatar da isar da lokaci amfani.
-
-
Tsawon tsarin kula da inganci
Cikakken tsari ISO 9000 ingancin tsarin, daga zane zuwa masana'antu, daga kafin tallace-tallace zuwa bayan tallace-tallace, cikakken tabbatar da samfurin inganci da lafiya.
-
-
Cikakken bayan tallace-tallace tallafi
A matsayinmu na mai ba da mafita, muna samar da sabis na fasaha da goyon bayan dukan rayuwar kayan aikin don kawar da damuwar masu amfani.